Fractography and failure mechanisms in static mode I and mode II delamination testing of unidirectional carbon reinforced composites [2009]
- Category:
- Artículos
- Authors:
- María Isabel Viña Olay , Jaime Aurelio Viña Olay , Antonio Argüelles Amado , Jorge Bonhomme González
- Date:
- 01 of January of 2009
- It Is a Part of:
- Polymer Testing